PFM:Ni-Cr-Mo the minimum requirements required biocompatibility, and overall efficacy. in ISO 22674. You can create frame- With over three decades of clinical works and crowns with greater service, VeraBond V has been proven to strength and less bulk. offer patients durability, comfort and safety. Prescribe VeraBond V with Numerous clinical studies and in vitro evaluations confirm and validate confidence. VeraBond V's corrosion resistance, Tensile Strength Yield Strength 120,000 (828) 83,500 (576) psi (MPa) Verabond V psi (MPa) 1 Vita Elongation Percent % 10 Vickers Hardness HV1 380 Density Color 8.1 White g/cm3 Coefficient of Expansion (@500°C) X10-6 13.8 Melting Range Composition 2,124-2,282 (1,162-1,250) mark of Vita Zahnfabrik Ni 74.8% Cr 12.7% Mo 9.0% Al, Be, Co °F (°C) 13