PFM:Ni-Cr-Mo
the minimum requirements required in ISO 22674. You can create frame- works and crowns with greater strength and less bulk.
Numerous clinical studies and in vitro evaluations confirm and validate VeraBond V's corrosion resistance,
biocompatibility, and overall efficacy. With over three decades of clinical service, VeraBond V has been proven to offer patients durability, comfort and safety. Prescribe VeraBond V
with confidence. 1 Vita mark of Vita Zahnfabrik
Strength psi (MPa)
Tensile Verabond V
120,000 (828)
Strength psi (MPa)
Yield
83,500 (576)
Elongation
Percent %
10
Hardness HV1
Vickers 380
Density g/cm3
8.1
Color White
Coefficient of
Expansion (@500°C) X10-6
13.8
Melting Range °F (°C)
2,124-2,282 (1,162-1,250)
Composition
Ni 74.8% Cr 12.7% Mo 9.0% Al, Be, Co