Aalba Dent

The Catalog Is Loading Now...

Issue link: https://aalbadent.uberflip.com/i/75931

Contents of this Issue

Navigation

Page 12 of 43

PFM:Ni-Cr-Mo the minimum requirements required in ISO 22674. You can create frame- works and crowns with greater strength and less bulk. Numerous clinical studies and in vitro evaluations confirm and validate VeraBond V's corrosion resistance, biocompatibility, and overall efficacy. With over three decades of clinical service, VeraBond V has been proven to offer patients durability, comfort and safety. Prescribe VeraBond V with confidence. 1 Vita mark of Vita Zahnfabrik Strength psi (MPa) Tensile Verabond V 120,000 (828) Strength psi (MPa) Yield 83,500 (576) Elongation Percent % 10 Hardness HV1 Vickers 380 Density g/cm3 8.1 Color White Coefficient of Expansion (@500°C) X10-6 13.8 Melting Range °F (°C) 2,124-2,282 (1,162-1,250) Composition Ni 74.8% Cr 12.7% Mo 9.0% Al, Be, Co 13

Articles in this issue

view archives of Aalba Dent - The Catalog Is Loading Now...